Introduction:

MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties-ultra high strength, toughness, ductility and outstanding corrosion resistance. The alloy is work-strengthened and aged to obtain strength levels of 260 to 300 ksi(1793-2068 MPa). HY MP35N alloy resists corrosion in hydrogen sulfide, salt water and other chloride solution, as well as the mineral acids(nitric, hydrochloric, sulfuric).In addition, it has exceptional resistance to crevice and stress corrosion cracking in sea water and other hostile environments.

    Category:

    Description

    UNS R30035/MP35N

    MP35N Material grades and equivalents:MP35N/UNS R30035/ W.Nr 2.4999/ AMS 5844/Allvac 35N

    Chemical composition:

    Weight%

    Ni

    Co

    Cr

    Mo

    Ti

    Fe

    Si

    Mn

    P

    B

    S

    C

    MP35N

    33

    Balance

    19

    9

    1

    1

    0.15

    0.15

    0.015

    0.01

    0.01

    0.025

    37

    21

    10.5

    Max

    Max

    Max

    Max

    Max

    Max

    Max

    Max

     

    Mechanical properties:

    MP35N Alloy

    Ultimate Tensile

    Strength

    0.2% Offset Yield

    Strength

    Elongation in

    4D

    Reduction of Area

    Hardness

    Shear

    Strength**

    Typical Properties

    of Solution Treated

    (Annealed)

    130 ksi(896 MPa)

    55 ksi(379 MPa)

    65%

    75%

    90 HRB

    Typical Properties

    of AMS 5844 Product after 4 Hour Age at 1050℉(556℃)

    290 ksi(2000 MPa)

    280 ksi(1931 MPa)

    10%

    45%

    51 HRC

    AMS 5844 Specification Requirements after Aging 4 Hours at 1000-1200℉

    (538-648℃)

    260 ksi(1795 MPa),min.

    230 ksi(1585 MPa),min.

    8%,min.

    35%,min.

    150 ksi(1034 Mpa),min.

    The above data are longitudinal properties.

    • Tensile properties will change depending on product size.

    • Not required by AMS 5844, but this is guaranteed shear strength.

    UNS R30035/MP35N alloy has the following characteristics:

    • MP35N alloy is a non-magnetic nickel-cobalt-chromium-molybdenum alloy with unique ultra-high tensile strength (up to 300ksi[2068MPa], good ductility and toughness and very good corrosion resistance. In addition, the alloy It also shows extraordinary resistance to vulcanization, high temperature oxidation and hydrogen embrittlement.

    Corrosion resistance of UNS R30035/MP35N:

    • MP35N has good resistance to sulfuration, high temperature oxidation, crispness, salt spray and most mineral acids. The alloy has excellent resistance to stress corrosion cracking under severe environments (-200 to +315) and high strength. The alloy also has extremely high resistance to local corrosion, such as pitting and crevice corrosion.

    UNS R30035/MP35N application areas:

    • MP35N alloy can be used for fasteners, springs, non-magnetic components and instrument parts in medical, seawater, oil and gas well, chemical and food processing environments.

    Specifications

    • UNS R30035

    • AMS 5758 – MP35N VIM-VAR Bar

      Solution heat treated @1900-1925°F for 4 to 8 hours

    • AMS 5844 – MP35N VIM-VAR Bar

      Solution heat treated @1900-1925°F for 4 to 8 hours and Work Strengthened

    • AMS 5845 – MP35N VIM-VAR Bar

      Solution heat treated @ 1900-1925°F for 4 to 8 hours, Work Strengthened & Aged @ 1000-1200°F for 4 hours

    • NACE MR0175

    • ASTM F-562 – Surgical Implant Applications

    • BS 7252-6 Surgical Implant Applications

    • ISO 5832-6 Surgical Implant Applications

    Shanghai HY Industry Co., Ltd has international first-class material production equipment such as high temperature alloy isothermal forging production line, CONSARC vacuum melting furnace, VAR vacuum arc remelting furnace etc., with strong professional ability and highly responsible management team. We are a member of China Application of nuclear energy materials, Member of the International Council of the Aeronautical Sciences,China Electronic Materials Industry Association Magnetic Materials Branch. Years of experience in special alloy. When you have superalloy material inquiry, please contact us without hesitation. Shanghai HY Industry Co., Ltd is Corrosion & fatigue nickel alloy professional manufacturer,We will provide you with sincere and thoughtful service.

    When you want to know more about our products, please contact us:

    https://hynickelalloy.com

      Your Country*

      Your Company*

      Your Name*

      Your Email*

      Your Message*