high temperature spring
Special alloy high temperature spring
-
Special alloy high temperature springs are springs that are made of special materials and have good elasticity when working in a high temperature environment.
Special alloy high temperature spring standard:
-
JB/T 6655–93,prEN 4590-2000,EN4168-2003,EN13906,EN10151 etc.
Production of special alloy high temperature spring
-
All kinds of high and low temperature resistant -200~+950° springs are made of special materials and are suitable for high and low temperature environments. High and low temperature spring products include 304, 631, GH 4169, GH 4145, Monel K500, Inconel 718, Inconel X750, etc.
Brief introduction of special alloy high temperature spring:
-
Special alloy high temperature springs are made of special materials and adapt to high temperature environments from -250 to +950°.
Types of special alloy high temperature springs:
-
High temperature resistant stainless steel springs, compression springs, high temperature resistant tension springs, high temperature resistant torsion springs, high temperature resistant mold springs, high temperature resistant disc springs, etc.
Common materials for special alloy high temperature springs:
-
The materials of special alloy high-temperature springs are generally CrV, CrSi, Inconel. The recommended maximum temperature of high-temperature alloy materials is 200℃~950℃. Choose the suitable material according to the requirements of use.
-
T631J1/T631 are used for heat-resistant springs and springs with high tensile strength after heat treatment;
-
630(17-4PH) stainless steel is precipitation, quenching, martensitic stainless steel, and this grade has high strength, hardness and corrosion resistance. After heat treatment, the mechanical properties of the product are more perfect and can reach a compressive strength of up to 1100-1300 mpa (160-190 ksi). This grade cannot be used at temperatures higher than 300°C (570F) or very low. It has good corrosion resistance to the atmosphere and diluted acids or salts. Its corrosion resistance is the same as 304 and 430. -
Special alloy high temperature spring 400~650° material adopts GH4169, GH4145, Monel K500, Inconel 718, Inconel X750, etc.