Description
Maraging 300
Material grades and equivalents: UNS K93120. UNS K93160/ W. Nr.WS 1.6354/WS 1.6358
Chemical Composition:
Weight% | C | Si | Mn | S | P | Co | Ni | Mo | Ti | Al | Fe |
Maraging 300 | 0.03 max | 0.10 max | 0.10 max | 0.010 max | 0.010 max | 8.0-9.5 | 18.0-19.0 | 4.6-5.2 | 0.55-0.80 | 0.05-0.15 | Bal |
Typical Mechanical Properties:
0.2 % Yield Strength ksi | Ultimate Tensile Strength ksi | Elongation in 4D(%) | Reduction of Area % | Hardness Rc |
120 | 150 | 16 | 70 | 30 |
280 | 290 | 8 | 40 | 52 |
Characteristic as below:
Maraging 300 alloy is a very high strength iron base, nickel , molybdenum, cobalt alloy. It may be age hardened to a strength level of 300 ksi ultimate with a hardness on the order of Rockwell C 53.
Processing conditions and application:
Maraging 300 is used for tooling, transmission shafts, autosport components and light aircraft landing gear.